| Passes German’s LGA Quality Test |
60,000 compression cycle of 1400 N roller showed a score of 96 out of 100 (a reading of more than 70 implies good quality) |
|
| Excellent Tensile Strength |
Napure latex achieves Elongation at Break at 275 which far exceeds the minimum requirement of 150 of MS679:1999 standards. |
|
 |
|
|
|
|
|
| |
|
|
| Passed Skin Irritation Test |
24 hour contact of NAPURE on abraded skin found no sign of irritation. |
|
| Passed Skin Sensitisation Test |
3 weeks induction of NAPURE on bare skin showed no sign of positive allergic reaction. |
|
NAPURE uses rubber chemicals that achieve well above the FDA approved standard - Low cost substitutes may emit harmful gases when heated. |
|